Not All Press Section Paper Breaks Are Caused by Press Felt or Equipment Problems

In the pulp and paper manufacturing process, paper breaks are a common production problem. However, if one assumes a malfunction must be caused by the pressure section equipment simply because a paper break occurred there, this often leads to incorrect conclusions.

In fact, a paper break in the press section does not necessarily mean that the press section equipment itself is faulty. Likewise, the fact that a press felt appears to be running straight does not necessarily mean that dewatering and sheet transfer are proceeding normally. Similarly, a low vacuum level does not necessarily mean that the press felt is clogged. These symptoms may be linked to a range of operating factors, and they call for further evaluation against the actual operating conditions.

Identify Where the Paper Break Occurs

In fact, “paper break” is just a general term. Did the paper break before being drawn in, fall off during the drawing process, or break only after it had entered the compression zone? Does the paper break occur on the operator side, the drive side, or in the middle? These details all help determine where the problem might lie.

If the paper sheet has already softened or shows signs of cracking along the edges before transfer, go back and check the dewatering effectiveness of the forming section and the paper’s wet strength.

If the sheet fails to adhere stably to the felt after leaving the forming fabric, or if it detaches from the press felt after adhering, special attention should be paid to the transfer process and the condition of the felt.

If the sheet has already entered the pressing zone smoothly and a paper break occurs afterward, it is necessary to further inspect the condition of the pressing zone, the sheet feed, and the drive operation.

Press Felt Condition Goes Beyond Alignment

When checking the press felt condition, do not focus only on its alignment. Also check for wrinkles, fuzzing, wear, joint defects, and edge damage. Pay attention to whether the press felt guide is operating too frequently.

How Paper Sheet Condition Reflects Press Felt Condition

When assessing the condition of the press felt, it is also necessary to analyze it alongside the appearance of the printed pages.

Even if the press felt hasn’t visibly shifted out of place, its breathability and water drainage may have already deteriorated.

For example, whether the sheet transfer is stable, whether the sheet drifts, has edges fall off, or wrinkles at the press inlet, and whether the condition of the sheet changes after passing through the press.

Interpreting Vacuum Readings in Actual Operating Conditions

If felt vacuum gradually drops before a paper break and sheet dewatering or transfer also deteriorates, inspect the press felt and vacuum system first.

However, a drop in vacuum level does not necessarily indicate that the press felt is clogged. It may also be related to issues with the water tank, piping, seals, drainage system, or abnormal measurement signals. Each item must be checked individually based on the on-site conditions.

show you about sun hong press felt sun hong press felt ready to deliver

Assessing Paper Breaks Through Felt Condition and Vacuum Performance

Identify the Paper Break Location

Record whether the paper break occurred before the suction transfer, during the sheet transfer, or near the pressure zone, and specify whether the abnormality first appeared on the operating side, the drive side, or in the middle of the web.

Check the Sheet Condition Before the Break

Before a paper break occurs, check whether the sheet shows signs of softening, edge loss, drifting, wrinkling, or localized tearing.

Check the Press Felt Condition

Check the press felt for any misalignment, wrinkles, or wear. Inspect the seams, cleaning, and drainage, and note whether the corrector is activating frequently.

Compare Vacuum Trends

Determine when the vacuum level begins to change, check the related equipment and measurement points, and see whether the change coincides with any sheet abnormalities.

Check Press Section Draw and Equipment Conditions

If the press felt, vacuum system, and sheet transfer all look normal, you still need to check further. Look at the speed differences between machine sections, the draw conditions, the running state of the rolls, and the drive feedback signals.

When the press felt vacuum drops gradually before a paper break, sheet moisture usually rises and transfer turns unstable. That pattern points to a break at the press inlet, so begin troubleshooting with the felt’s dewatering capacity and its vacuum system.

If the vacuum stays stable and the press felt runs smoothly, but the draw fluctuates right before a break, the felt alone is unlikely to be the cause. Focus instead on the speed differences between sections and the drive feedback signals.

Confirm That the Problem Has Been Resolved

After the inspection and adjustments, seeing the paper web reattached is not enough. Keep monitoring the felt positions, the vacuum trends, the sheet transfer, and the press section operation. When all of these readings return to their normal ranges, the problem is genuinely solved.